Preparation and electrical properties of TbSb films


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

Thin polycrystalline TbSb films have been grown by thermal evaporation in vacuum from two separate sources on glass-ceramic, sapphire, and single-crystal silicon substrates. The substrate material has been shown to have no significant effect on the phase composition and crystallinity of the films. The optimal substrate temperature is 1120–1145 K. The films have a cubic structure (NaCl type), their composition is 49 ± 0.01 at % Tb + 50.1 ± 0.01 at % Sb, and their components are uniformly distributed both on the surface and in the bulk of the films. The resistivity, Hall coefficient, and thermoelectric power of the films have been measured as functions of temperature in the temperature range 95–700 K. It has been shown that charge carriers in the films are electrons, with a concentration of ~1026 m–3 and mobility of ~10–3 m2/(V s). According to the electrical measurements, TbSb is a semimetal.

作者简介

Z. Jabua

Department of Physics

编辑信件的主要联系方式.
Email: Z.Jabua@hotmail.com
格鲁吉亚, Kostava str. 77, Tbilisi, 0175

补充文件

附件文件
动作
1. JATS XML

版权所有 © Pleiades Publishing, Ltd., 2017