High-Pressure Magnetic and Transport Properties of Zn0.1Cd0.9GeAs2 + n wt % MnAs (n = 10 or 15) Nanocomposites


Citar

Texto integral

Acesso aberto Acesso aberto
Acesso é fechado Acesso está concedido
Acesso é fechado Somente assinantes

Resumo

The magnetic susceptibility χ(T) of Zn0.1Cd0.9GeAs2 + n wt % MnAs (n = 10 or 15) ferromagnetic nanocomposites with a Curie temperature TC = 310 K has been measured as a function of temperature in the temperature range 270–350 K, and their resistivity ρ(p), Hall coefficient RH(p), and magnetization M(p) have been measured as functions of pressure near room temperature. The materials have been shown to undergo a pressure-induced ferromagnetic-to-paramagnetic phase transition, accompanied by a semiconductor–metal phase transition, at a hydrostatic pressure p ≈ 3.2 GPa and room temperature.

Sobre autores

R. Arslanov

Amirkhanov Institute of Physics, Dagestan Scientific Center, Russian Academy of Sciences

Autor responsável pela correspondência
Email: arslanovr@gmail.com
Rússia, ul. Yaragskogo 94, Makhachkala, Dagestan, 367015

T. Arslanov

Amirkhanov Institute of Physics, Dagestan Scientific Center, Russian Academy of Sciences

Email: arslanovr@gmail.com
Rússia, ul. Yaragskogo 94, Makhachkala, Dagestan, 367015

U. Zalibekov

Amirkhanov Institute of Physics, Dagestan Scientific Center, Russian Academy of Sciences

Email: arslanovr@gmail.com
Rússia, ul. Yaragskogo 94, Makhachkala, Dagestan, 367015

I. Fedorchenko

Kurnakov Institute of General and Inorganic Chemistry, Russian Academy of Sciences

Email: arslanovr@gmail.com
Rússia, Leninskii pr. 31, Moscow, 119991

Arquivos suplementares

Arquivos suplementares
Ação
1. JATS XML

Declaração de direitos autorais © Pleiades Publishing, Inc., 2019