Europium-doped YVO4 phosphors have been synthesized using microwave radiation of 700 W power. The uniformity and high rate of microwave heating, as well as “nonthermal” effects of microwave radiation, considerably accelerate the decomposition of precursors and YVO4:Eu3+ synthesis. The europium concentration was varied from 1 to 8 at %. The luminescence intensity of YVO4:Eu3+ was shown to depend on Eu3+ concentration, with a maximum at 8 at % Eu3+. According to transmission electron microscopy data, the synthesized phosphors consist of nanoparticles 6 to 8 nm in size, with an appreciable degree of agglomeration.

Авторлар туралы

E. Tomina

Voronezh State University

Хат алмасуға жауапты Автор.
Email: inorg@chem.vsu.ru
Ресей, Universitetskaya pl. 1, Voronezh, 394006

B. Sladkopevtsev

Voronezh State University

Email: inorg@chem.vsu.ru
Ресей, Universitetskaya pl. 1, Voronezh, 394006

V. Mittova

Burdenko State Medical University

Email: inorg@chem.vsu.ru
Ресей, Studencheskaya ul. 10, Voronezh, 394036

M. Knurova

Voronezh State University

Email: inorg@chem.vsu.ru
Ресей, Universitetskaya pl. 1, Voronezh, 394006

A. Latyshev

Voronezh State University

Email: inorg@chem.vsu.ru
Ресей, Universitetskaya pl. 1, Voronezh, 394006

I. Mittova

Voronezh State University

Email: inorg@chem.vsu.ru
Ресей, Universitetskaya pl. 1, Voronezh, 394006

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Pleiades Publishing, Ltd., 2016