Relative lengthening of ZrO2 in the temperature range of 1200–2700 K
- Authors: Kostanovskiy A.V.1, Zeodinov M.G.1, Kostanovskaya M.E.1, Pronkin A.A.1, Borodina T.I.1
-
Affiliations:
- Joint Institute for High Temperatures
- Issue: Vol 55, No 6 (2017)
- Pages: 942-944
- Section: Short Communications
- URL: https://journals.rcsi.science/0018-151X/article/view/157415
- DOI: https://doi.org/10.1134/S0018151X17060116
- ID: 157415
Cite item
Abstract
Results from the experimental investigation of the relative lengthening and mean thermal coefficient of the linear expansion of zirconium dioxide in the 1200–2700 K range are presented.
About the authors
A. V. Kostanovskiy
Joint Institute for High Temperatures
Author for correspondence.
Email: Kostanovskiy@gmail.com
Russian Federation, Moscow, 125412
M. G. Zeodinov
Joint Institute for High Temperatures
Email: Kostanovskiy@gmail.com
Russian Federation, Moscow, 125412
M. E. Kostanovskaya
Joint Institute for High Temperatures
Email: Kostanovskiy@gmail.com
Russian Federation, Moscow, 125412
A. A. Pronkin
Joint Institute for High Temperatures
Email: Kostanovskiy@gmail.com
Russian Federation, Moscow, 125412
T. I. Borodina
Joint Institute for High Temperatures
Email: Kostanovskiy@gmail.com
Russian Federation, Moscow, 125412
Supplementary files