Relative lengthening of ZrO2 in the temperature range of 1200–2700 K
- Авторы: Kostanovskiy A.V.1, Zeodinov M.G.1, Kostanovskaya M.E.1, Pronkin A.A.1, Borodina T.I.1
-
Учреждения:
- Joint Institute for High Temperatures
- Выпуск: Том 55, № 6 (2017)
- Страницы: 942-944
- Раздел: Short Communications
- URL: https://journals.rcsi.science/0018-151X/article/view/157415
- DOI: https://doi.org/10.1134/S0018151X17060116
- ID: 157415
Цитировать
Аннотация
Results from the experimental investigation of the relative lengthening and mean thermal coefficient of the linear expansion of zirconium dioxide in the 1200–2700 K range are presented.
Об авторах
A. Kostanovskiy
Joint Institute for High Temperatures
Автор, ответственный за переписку.
Email: Kostanovskiy@gmail.com
Россия, Moscow, 125412
M. Zeodinov
Joint Institute for High Temperatures
Email: Kostanovskiy@gmail.com
Россия, Moscow, 125412
M. Kostanovskaya
Joint Institute for High Temperatures
Email: Kostanovskiy@gmail.com
Россия, Moscow, 125412
A. Pronkin
Joint Institute for High Temperatures
Email: Kostanovskiy@gmail.com
Россия, Moscow, 125412
T. Borodina
Joint Institute for High Temperatures
Email: Kostanovskiy@gmail.com
Россия, Moscow, 125412
Дополнительные файлы