The article presents the results of the influence of temperature and deformation during snap temper of structural steel 38ХН3МФА. It is shown that 300°С and 500°С deformation temperatures of 300 and 500° significantly increases the durability characteristics, but decreases the flexibility. The subsequent after deformation snap temper at a temperature 560°С has a positive effect on the mechanical properties complex.

作者简介

A. Prokhorova

Moscow State University of Mechanical Engineering (MAMI)

Email: kafmaterialy@mail.ru
Ph.D.; +7 (906) 096-48-55

A. Borisova

Moscow State University of Mechanical Engineering (MAMI)

Email: kafmaterialy@mail.ru
+7 (906) 096-48-55

参考

  1. Металловедение и термическая обработка стали. В 3 т. - М. Т. 2 / Бернштейн М.Л., Рахштадт А.Г.: Металлургия, 1983 - 368 с.
  2. Современные направления стабилизации прочности и долговечности в машиностроительной продукции / Зинченко В.М., Маневский С.Е., Прохорова А.И.: Технология металлов, 2012. №10 - с. 12 - 18.
  3. Деформационное упрочнение закаленных конструкционных сталей / Васильева А.Г.: М. Машиностроение, 1981 - 232 с.
  4. Перераспределение углерода при деформации закаленной конструкционной стали / Корнет Е.В., Иванов Ю.Ф., Коновалов С.В., Громов В.Е.: Фундаментальные проблемы современного материаловедения. 2009. № 1 - с. 101 - 105.
  5. Закаленная конструкционная сталь: структура и механизмы упрочнения / Иванов Ю.Ф., Корнет Е.В., Громов В.Е.: Новокузнецк. Изд-во СибГИУ, 2010 - 173 с.

版权所有 © Prokhorova A.I., Borisova A.S., 2014

Creative Commons License
此作品已接受知识共享署名-非商业性使用-禁止演绎 4.0国际许可协议的许可。

##common.cookie##