Optical and Structural Properties of Indium Sulfide Thin Film Produced by CBD Method


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

Indium sulfide thin films were prepared by chemical bath deposition (CBD) method on a glass substrate at a sedimentation time of about 45 min. The films were grown at different bath temperature as 30, 55, 70 and 85°C. The crystallinity, nanostructures and morphology of the prepared films have been investigated by using X-ray diffraction (XRD), scanning electron microscopy (SEM) and atomic force microscopy (AFM) analyses. Optical reflectance of layers was measured in the energy range of 1.5–5.5 eV by spectrophotometer instrument. Kramers–Kronig relations were used to calculate the optical constants. The X-ray diffraction spectrum showed that by increasing in growth temperature, crystalline structure was changed. According to the atomic force microscope images, with increasing growth temperature, roughness increases consistently. Optical results revealed that the highest optical band gap of 3.4 eV and the highest transmittance of ~90% were achieved at higher deposition temperature (85°C).

Авторлар туралы

Parisa Esmaili

Plasma Physics Research Center, Science and Research Branch, Islamic Azad University

Хат алмасуға жауапты Автор.
Email: p.esmaili89@yahoo.com
Иран, Tehran

Haleh Kangarlou

Department of Physics, Urmia Branch, Islamic Azad University

Email: p.esmaili89@yahoo.com
Иран, Urmia

Mahmood Ghorannevis

Plasma Physics Research Center, Science and Research Branch, Islamic Azad University

Email: p.esmaili89@yahoo.com
Иран, Tehran

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Pleiades Publishing, Ltd., 2019