Composite Materials with Ultrahigh-Molecular-Weight Polyethylene and Boron Synthesized via Polymerization in situ

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

Composite materials made of ultrahigh-molecular-weight polyethylene (UHMWPE) and boron have been synthesized using polymerization filling (polymerization in situ), varying the boron content in a wide range from, 10 to 75 vol %. The behavior of synthesized composites during deformation under compression depending on the degree of filling has been studied, and it has been determined that composites with a boron content of about 45 vol % have the maximum value for Young’s modulus, and increases in stress values at offset yield strength under compression is observed up to the filler content of 52 vol %. Based on the analysis of the stress–strain curves under compression, it can be asserted that, even at high degrees of filling, UHMWPE–boron composites retain plastic deformation.

Авторлар туралы

I. Maklakova

Semenov Institute of Chemical Physics

Хат алмасуға жауапты Автор.
Email: maklakosha@yandex.ru
Ресей, Moscow, 119991

V. Grinev

Semenov Institute of Chemical Physics

Email: maklakosha@yandex.ru
Ресей, Moscow, 119991

O. Kudinova

Semenov Institute of Chemical Physics

Email: maklakosha@yandex.ru
Ресей, Moscow, 119991

V. Krasheninnikov

Semenov Institute of Chemical Physics

Email: maklakosha@yandex.ru
Ресей, Moscow, 119991

A. Gorenberg

Semenov Institute of Chemical Physics

Email: maklakosha@yandex.ru
Ресей, Moscow, 119991

L. Novokshonova

Semenov Institute of Chemical Physics

Email: maklakosha@yandex.ru
Ресей, Moscow, 119991

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Pleiades Publishing, Ltd., 2018