Cycling Performance at Li7La3Zr2O12|Li Interface


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

Cyclability of the Li|Li7La3Zr2O12 interface was tested by voltammetry under externally applied potential difference. It was found that the solid electrolyte synthesized in the study contains a minor amount of an impurity in the form of lithium carbonate. This impurity forms, when brought in contact with metallic lithium, carbon that pierces the whole volume of the ceramic separator and produces a channel for a flow of electrons through the material, which leads to a poor cyclability of the solid electrolyte. A possible way to solve the given problem is via a purposeful replacement of the carbonate in the intergrain space of Li7La3Zr2O12 with another crystalline or glassy plasticizer that possesses an acceptable unipolar lithium conductivity (no less than 10–6 S cm–1) and forms, when brought in contact with metallic lithium, no electrically conducting compound or a compound capable of reversibly intercalating/deintercalating lithium.

作者简介

K. Druzhinin

Institute of High-Temperature Electrochemistry, Ural Branch; Ural Federal University Named after the First President of Russia B.N.Yeltsin

编辑信件的主要联系方式.
Email: druzginin@mail.ru
俄罗斯联邦, ul. S. Kovalevskoi 22, Yekaterinburg, 620219; ul. Mira 19, Yekaterinburg, 620002

P. Shevelin

Institute of High-Temperature Electrochemistry, Ural Branch

Email: druzginin@mail.ru
俄罗斯联邦, ul. S. Kovalevskoi 22, Yekaterinburg, 620219

E. Il’ina

Institute of High-Temperature Electrochemistry, Ural Branch

Email: druzginin@mail.ru
俄罗斯联邦, ul. S. Kovalevskoi 22, Yekaterinburg, 620219

补充文件

附件文件
动作
1. JATS XML

版权所有 © Pleiades Publishing, Ltd., 2018