A process was developed for chromate-free passivation of zinc-plated surfaces via formation of conversion silicon-containing coatings on these surfaces. The passivation performed in a solution containing 20–35 g L−1 sodium metasilicate, 0.2–0.5 g L−1 phosphonic acid, 20–30 mL L−1 H2O2, 200–500 mg L−1 saccharine, and 4–10 mg L−1 potassium pyrophosphate at pH 2.0–2.5 and temperature of 18–25°C in the course of 4 min. A warming-up of the solution to 40°C is allowed. The developed silicon-containing passivating coatings on zinc-plated steel details are comparable in corrosion resistance and protective capacity with iridescent chromate coatings, but, in contrast to the latter, sustain a thermal shock without deterioration of their protective characteristics and are more wear resistant.

Авторлар туралы

A. Abrashov

Mendeleev University of Chemical Technology of Russia

Хат алмасуға жауапты Автор.
Email: abr-aleksey@yandex.ru
Ресей, Moscow, 125047

N. Grigoryan

Mendeleev University of Chemical Technology of Russia

Email: abr-aleksey@yandex.ru
Ресей, Moscow, 125047

E. Zheludkova

Mendeleev University of Chemical Technology of Russia

Email: abr-aleksey@yandex.ru
Ресей, Moscow, 125047

T. Vagramyan

Mendeleev University of Chemical Technology of Russia

Email: abr-aleksey@yandex.ru
Ресей, Moscow, 125047

N. Asnis

Mendeleev University of Chemical Technology of Russia

Email: abr-aleksey@yandex.ru
Ресей, Moscow, 125047

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Pleiades Publishing, Ltd., 2019