Influence of electrospark discharge parameters on roughness and microabrasive wear of steel 45 surface after ESA by TiC-based electrodes
- Авторлар: Nikolenko S.V.1, Verkhoturov A.D.2, Syui N.A.1, Kuz’michev E.N.3
- 
							Мекемелер: 
							- Institute of Materials Science
- Institute of Water and Ecological Problems
- Far Eastern State Transport University
 
- Шығарылым: Том 52, № 4 (2016)
- Беттер: 342-349
- Бөлім: Article
- URL: https://journals.rcsi.science/1068-3755/article/view/229773
- DOI: https://doi.org/10.3103/S1068375516040098
- ID: 229773
Дәйексөз келтіру
Аннотация
The influence of the parameters of electrospark discharge and electrode materials for electrospark alloying using the additives of boron-containing mineral raw material on the characteristics of microgeometry and microabrasive wear of the coating surface is investigated. It is found that the longer is the electrospark duration (from 20 to 80 μs), the higher is the surface roughness. The introduction of 1–2% of boron-containing raw material improves physicochemical properties of the alloyed layer, reduces the roughness, and increases the wear resistance.
Авторлар туралы
S. Nikolenko
Institute of Materials Science
							Хат алмасуға жауапты Автор.
							Email: nikola960@mail.ru
				                					                																			                												                	Ресей, 							ul. Tikhookeanskaya 153, Khabarovsk, 680042						
A. Verkhoturov
Institute of Water and Ecological Problems
														Email: nikola960@mail.ru
				                					                																			                												                	Ресей, 							ul. Kim-Yu-Chena 65, Khabarovsk, 680000						
N. Syui
Institute of Materials Science
														Email: nikola960@mail.ru
				                					                																			                												                	Ресей, 							ul. Tikhookeanskaya 153, Khabarovsk, 680042						
E. Kuz’michev
Far Eastern State Transport University
														Email: nikola960@mail.ru
				                					                																			                												                	Ресей, 							ul. Serysheva 47, Khabarovsk, 680021						
Қосымша файлдар
 
				
			 
						 
						 
						 
					 
						 
									 
  
  
  
  
  Мақаланы E-mail арқылы жіберу
			Мақаланы E-mail арқылы жіберу  Ашық рұқсат
		                                Ашық рұқсат Рұқсат берілді
						Рұқсат берілді Тек жазылушылар үшін
		                                		                                        Тек жазылушылар үшін
		                                					