Production of high-carbon ferrochrome from dry-quenched semicoke


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

The quenching of semicoke by saturated steam (heating-gas temperature 550°C) is described. The working-moisture content Wr in the semicoke is 3.0–6.7% for the new quenching method. As a reducing agent, semicoke has good characteristics: relatively low ash content (Ad = 7.1%), low sulfur content (Sd = 0.13%) and phosphorus content (Pd = 0.029%), and high reactivity (\({K_{C{O_2}}}\) = 4.0 cm3/g s) and electrical resistivity (ρ > 1.9 × 106 Ω cm). In tests, dry-quenched semicoke performs well in the production of high-carbon ferrochrome: decreased power consumption; increased furnace productivity; decreased consumption of chromium ore; and decreased sulfur content in the ferrochrome when Karaganda coal is completely reduced by the semicoke. The optimal semicoke content in the batch is up to 50 kg.

作者简介

V. Strakhov

Kuznetsk Center

编辑信件的主要联系方式.
Email: vuhin2013@yandex.ru
俄罗斯联邦, ul. Klimasenko 19, Novokuznetsk, 654040

V. Medyanik

Leninsk-Kuznetsk Semicoking Plant

Email: vuhin2013@yandex.ru
俄罗斯联邦, ul. Voikova 1, Leninsk-Kuznetsk, 652515

L. Malinovskaya

Leninsk-Kuznetsk Semicoking Plant

Email: vuhin2013@yandex.ru
俄罗斯联邦, ul. Voikova 1, Leninsk-Kuznetsk, 652515

A. Tsernikel

Serov Ferro-Alloy Plant

Email: vuhin2013@yandex.ru
俄罗斯联邦, ul. Nakhabina 1, Serov, 624992

I. Veselovsky

Serov Ferro-Alloy Plant

Email: vuhin2013@yandex.ru
俄罗斯联邦, ul. Nakhabina 1, Serov, 624992

补充文件

附件文件
动作
1. JATS XML

版权所有 © Allerton Press, Inc., 2016