Resumo

Laboratory research indicates that the gross calorific value of blast-furnace coke is greatest for batch with Ro = 0.913–0.942%, Vdaf = 30.9–31.0%, Cdaf = 83.8%, Hdaf = 5.01–5.02%, and \({\text{O}}_{d}^{{daf}}\) = 8.42–8.45%. Increase in the packing density of coking batch of consistent quality from 800 to 1150 kg/m3 increases the gross calorific value of blast-furnace coke by 0.05–0.12 MJ/kg.

Sobre autores

I. Miroshnichenko

ChAO MK Azovstal

Autor responsável pela correspondência
Email: igor.miroshnichenko@azovstal.com.ua
Ucrânia, Mariupol, 87500

D. Miroshnichenko

Kharkov Polytechnic Institute

Autor responsável pela correspondência
Email: dvmir79@gmail.com
Ucrânia, Kharkov, 61002

I. Shulga

Ukrainian State Coal-Chemistry Institute (UKhIN)

Autor responsável pela correspondência
Email: ko@ukhin.org.ua
Ucrânia, Kharkov, 61023

Y. Balaeva

Ukrainian State Coal-Chemistry Institute (UKhIN)

Autor responsável pela correspondência
Email: ys.balaeva@gmail.com
Ucrânia, Kharkov, 61023


Declaração de direitos autorais © Allerton Press, Inc., 2019

Este site utiliza cookies

Ao continuar usando nosso site, você concorda com o procedimento de cookies que mantêm o site funcionando normalmente.

Informação sobre cookies