Sorption of Rhenium from Sulfuric Acid Solutions with Trialkylamine-Containing Impregnates
- Авторлар: Troshkina I.D.1, Veselova O.A.1, Vatsura F.Y.1, Zakharyan S.V.2, Serikbay A.U.2
-
Мекемелер:
- Mendeleev University of Chemical Technology of Russia
- TOO Kazgipromed
- Шығарылым: Том 58, № 6 (2017)
- Беттер: 608-613
- Бөлім: Metallurgy of Rare and Noble Metals
- URL: https://journals.rcsi.science/1067-8212/article/view/226368
- DOI: https://doi.org/10.3103/S106782121706013X
- ID: 226368
Дәйексөз келтіру
Аннотация
The sorption of rhenium (VII) from sulfuric acid solutions with impregnates based on macroporous polymeric carriers (copolymers of styrene with divinylbenzene, a weakly acidic cation-exchange resin), which contain technical trialkylamine (TAA), is investigated in batch conditions. Equilibrium and kinetic characteristics of sorption of rhenium with the K-TAA impregnate based on macroporous cationite having the best capacitive characteristics with respect to rhenium are found. The maximal distribution coefficient of rhenium in the K-TAA impregnate is observed during sorption from solutions with pH 2. The sorption isotherm of rhenium is described by the Langmuir equation with constant K = 29 ± 2 mL/g. Integrated kinetic curves of sorption are found by the method of a limited solution volume at various temperatures and effective diffusion coefficients of rhenium in an impregnate, which are equal to 3.8 × 10–11 (295 K) and 1.3 × 10–10 (308 K) m2/s, are calculated allowing to the half-transformation time. Processing the kinetic data by linearization according to equations of models of the pseudo-first, pseudo-second, internal diffusion, and Elovich showed that kinetic curves are described with the highest degree of correlation by pseudo-second-order equations with rate constants 0.00056 (295 K) and 0.00059 (308 K) g mg–1 min–1. The apparent activation energy of sorption of rhenium of 39 ± 2 kJ/mol is calculated according to the Arrhenius equation. The K-TAA impregnate is approved for the sorption of rhenium from the eluate formed during the desorption of rhenium from the weakly basic anion-exchange resin (Purolite A170) preliminarily saturated with rhenium from a productive leaching solution of processing products of rhenium-containing off-balance copper-sulfide ores with a complex composition.
Авторлар туралы
I. Troshkina
Mendeleev University of Chemical Technology of Russia
Хат алмасуға жауапты Автор.
Email: tid@rctu.ru
Ресей, Moscow, 125047
O. Veselova
Mendeleev University of Chemical Technology of Russia
Email: tid@rctu.ru
Ресей, Moscow, 125047
F. Vatsura
Mendeleev University of Chemical Technology of Russia
Email: tid@rctu.ru
Ресей, Moscow, 125047
S. Zakharyan
TOO Kazgipromed
Email: tid@rctu.ru
Қазақстан, Karaganda, 100009
A. Serikbay
TOO Kazgipromed
Email: tid@rctu.ru
Қазақстан, Karaganda, 100009
Қосымша файлдар