Effect of scandium on the phase composition and hardening of casting aluminum alloys of the Al–Ca–Si system


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

The phase composition of the Al–Ca–Si–Sc system is investigated in aluminum corner uisng computational (Thermo-Calc) and experimental (optical microscopy, scanning electron microscopy, and electron probe microanalysis) methods. The influence of annealing on the structure and hardness of alloys containing 0.3 wt % Sc is investigated in the region up to 550°C. It is shown that the maximum in the hardening curve caused by the isolation of nanoparticles of the Al3Sc (L12) is attained after annealing at temperatures of 300–350°C in alloys belonging to the phase region (Al) + Al4Ca + Al2Si2Ca ((Al) is the aluminum-based solid solution). Scandium completely enters the (Al) composition in alloys of this region, while the silicon concentration is minimal in it. On the other hand, hardening is almost absent in alloys from the (Al) + (Si) + Al2Si2Ca phase region. The possibility in principle to form the casting alloys based on the (Al) + Al4Ca + Al2Si2Ca eutectic hardened without quenching is substantiated.

作者简介

N. Belov

National University of Science and Technology MISiS

编辑信件的主要联系方式.
Email: nikolay-belov@yandex.ru
俄罗斯联邦, Moscow, 119049

E. Naumova

Bauman State Technical University

Email: nikolay-belov@yandex.ru
俄罗斯联邦, Moscow, 107005

V. Doroshenko

National University of Science and Technology MISiS

Email: nikolay-belov@yandex.ru
俄罗斯联邦, Moscow, 119049

T. Bazlova

National University of Science and Technology MISiS

Email: nikolay-belov@yandex.ru
俄罗斯联邦, Moscow, 119049

补充文件

附件文件
动作
1. JATS XML

版权所有 © Allerton Press, Inc., 2016