Optimization of fluorination of the tungsten powder with fluorine in a reactor with an immobile layer with the provision of green requirements


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

The computational procedures to model the fluorination of the tungsten powder with fluorine and condensation of formed WF6, which describe the available experimental data satisfactorily, are developed using physicochemical foundations of processes. With their help, the equipment sizes and process parameters of the two-stage fluorination of the tungsten powder with fluorine with the condensation of liquid WF6 after each stage at 2.5–3.0°C are optimized. The possibility of fabricating WF6 with productivity of 5.23, 6.53, and 7.83 kg/h in reactors 200, 300, and 360 mm in diameter, respectively, at 300–350°C without the forced cooling of the highest heat-beat first fluorination setup is shown. The completeness of fluorine usage higher than 99.99% is attained in this case, while the amount of harmful gases (F2, WF6) leaving the process chain does not exceed their maximal permissible concentrations already in the vent gas volume. Recommendations for the organization of the fluorination production process of the tungsten powder are given.

Авторлар туралы

Yu. Korolev

Scientific-and-Technical Association “Powder Metallurgy”

Хат алмасуға жауапты Автор.
Email: stamp@mail.ru
Ресей, Moscow, 105005

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Allerton Press, Inc., 2016