Structure, Linear Thermal Expansion Coefficient, and Electrical Conductivity of Y0.9Ca0.1Cr1 – уCoуO3 (у = 0–0.9) Perovskites
- Авторы: Gil’derman V.K.1, Antonov B.D.1
-
Учреждения:
- Institute of High-Temperature Electrochemistry, Ural Branch, Russian Academy of Sciences
- Выпуск: Том 64, № 3 (2019)
- Страницы: 474-478
- Раздел: Nanomaterials and Ceramics
- URL: https://journals.rcsi.science/1063-7745/article/view/194004
- DOI: https://doi.org/10.1134/S1063774519030076
- ID: 194004
Цитировать
Аннотация
The structure, thermal expansion coefficient, and electrical conductivity of Y0.9Ca0.1Cr1 – уCoуO3 (у = 0–0.9) compounds with the perovskite structure have been investigated in air in the temperature range of 100–1000°С. The linear thermal expansion coefficient of Y1 – хCaхCr1 – уCoуO3 lies in the range of (8.77–16.1) × 10–6 K–1. The maximum electrical conductivity is attained for the Y0.9Ca0.1Cr0.6Co0.4O3 composition. It is shown that the electrical conductivity at low (25–270°С) temperatures and weak substitution of cobalt for chromium is mainly due to the hopping of one electron hole from Cr4+ to Cr3+. At high (565–1000°С) temperatures and cobalt contents, this conductivity mechanism is supplemented with the conductivity caused by the hopping of an electron hole from Cо3+ to Cо2+.
Об авторах
V. Gil’derman
Institute of High-Temperature Electrochemistry, Ural Branch, Russian Academy of Sciences
Email: B.Antonov@ihte.uran.ru
Россия,
Yekaterinburg, 620990
B. Antonov
Institute of High-Temperature Electrochemistry, Ural Branch, Russian Academy of Sciences
Автор, ответственный за переписку.
Email: B.Antonov@ihte.uran.ru
Россия,
Yekaterinburg, 620990
Дополнительные файлы