Effect of the rate of cooling tungsten heavy alloys of the W–Ni–Fe type from the sintering temperature on the formation of their physico-mechanical properties
- 作者: Andreiev I.V.1
-
隶属关系:
- Bakul Institute for Superhard Materials
- 期: 卷 38, 编号 3 (2016)
- 页面: 185-189
- 栏目: Production, Structure, Properties
- URL: https://journals.rcsi.science/1063-4576/article/view/185565
- DOI: https://doi.org/10.3103/S1063457616030059
- ID: 185565
如何引用文章
详细
The effect of the conditions of cooling after the liquid-phase sintering of tungsten heavy metals have been studied. It has been found that to attain a high ductility of the tungsten heavy metal, the rate of cooling from the sintering temperature should afford removal of the major part of hydrogen, which was dissolved in the alloy volume in the temperature range of the liquid phase existence.