Experimental Investigation of Tellurium Corrosion of Nickel-Molybdenum Alloys in Molten Lithium-, Beryllium-, and Uranium-Fluoride Salts
- Authors: Ignat’ev V.V.1, Surenkov A.I.1, Gnidoi I.P.1, Uglov V.S.1, Konakov S.A.1
-
Affiliations:
- National Research Center Kurchatov Institute
- Issue: Vol 120, No 6 (2016)
- Pages: 397-402
- Section: Article
- URL: https://journals.rcsi.science/1063-4258/article/view/247768
- DOI: https://doi.org/10.1007/s10512-016-0148-1
- ID: 247768
Cite item
Abstract
The test results on the compatibility of special nickel-molybdenum alloys with a fuel salt with the composition 71LiF–27BeF2–2UF4, containing tellurium additive, at temperature 760–800°C and controlled values of the redox potential, determined by the ratio [U(IV)]/[U(III)] = 30, 60, and 90, are colligated. A comparison of corrosion tests of the alloys with fuel salt with the chosen composition confi rmed the threshold character of the dependence of the intercrystallite corrosion intensity on the ratio [U(IV)]/[U(III)] and melt temperature. The domestic alloy KhN80MTYu is recommended for further study as the main structural material of the reactor loop of a molten salt reactor with the maximum temperature of the fuel salt 750–800°C.
About the authors
V. V. Ignat’ev
National Research Center Kurchatov Institute
Email: j-atomicenergy@yandex.ru
Russian Federation, Moscow
A. I. Surenkov
National Research Center Kurchatov Institute
Email: j-atomicenergy@yandex.ru
Russian Federation, Moscow
I. P. Gnidoi
National Research Center Kurchatov Institute
Email: j-atomicenergy@yandex.ru
Russian Federation, Moscow
V. S. Uglov
National Research Center Kurchatov Institute
Email: j-atomicenergy@yandex.ru
Russian Federation, Moscow
S. A. Konakov
National Research Center Kurchatov Institute
Email: j-atomicenergy@yandex.ru
Russian Federation, Moscow
Supplementary files