Catalytic Oxidation of Trace Quantities of Hydrogen in Tritium-Containing Gas Flows in the Event of a Fire at Nuclear Facilities
- 作者: Ivanova A.S.1, Bukin A.N.1, Marunich S.A.1, Pak Y.S.1, Rozenkevich M.B.1
-
隶属关系:
- Mendeleev Russian Chemical-Technological University
- 期: 卷 120, 编号 2 (2016)
- 页面: 127-133
- 栏目: Article
- URL: https://journals.rcsi.science/1063-4258/article/view/247597
- DOI: https://doi.org/10.1007/s10512-016-0106-y
- ID: 247597
如何引用文章
详细
The effect of the fume gases, produced when the insulation of chlorine-free cables burns, on the catalytic activity of hydrophobic low-temperature and hydrophilic high-temperature platinum catalysts of hydrogen oxidation, which are to be used in the ventilation-gas detritization system. The temperature regime for the combustion of cables in the presence of an oxygen deficiency is determined and the semiquantitative composition of the products formed is obtained. Upon exposure to the fume gas flow at room temperature the experimental samples of the catalysts were almost completely poisoned. At the initial temperature 473 K of a hydrophilic catalyst thermal activation of the catalyst occurs in the presence of fume gases.
作者简介
A. Ivanova
Mendeleev Russian Chemical-Technological University
Email: j-atomicenergy@yandex.ru
俄罗斯联邦, Moscow
A. Bukin
Mendeleev Russian Chemical-Technological University
Email: j-atomicenergy@yandex.ru
俄罗斯联邦, Moscow
S. Marunich
Mendeleev Russian Chemical-Technological University
Email: j-atomicenergy@yandex.ru
俄罗斯联邦, Moscow
Yu. Pak
Mendeleev Russian Chemical-Technological University
Email: j-atomicenergy@yandex.ru
俄罗斯联邦, Moscow
M. Rozenkevich
Mendeleev Russian Chemical-Technological University
Email: j-atomicenergy@yandex.ru
俄罗斯联邦, Moscow
补充文件