Quasi-wave shape of an interface upon explosion welding (copper–tantalum, copper–titanium)


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

The interface relief of copper–titanium compounds and its evolution upon the intensification of explosion welding are investigated. Typical structures are revealed: splashes, waves consisting of ledges, interrupted waves, and transient states generated by interrupted waves combined into bands. The effect the mutual solubility of the initial elements has on the formation of a welded joint’s structure is determined. Intermetallic compounds are detected both on ledge surfaces and inside areas of local melting.

作者简介

M. Pushkin

Mikheev Institute of Metal Physics, Ural Branch

编辑信件的主要联系方式.
Email: limon.5ddd@yandex.ru
俄罗斯联邦, Yekaterinburg, 620999

A. Inozemtsev

Mikheev Institute of Metal Physics, Ural Branch

Email: limon.5ddd@yandex.ru
俄罗斯联邦, Yekaterinburg, 620999

B. Greenberg

Mikheev Institute of Metal Physics, Ural Branch

Email: limon.5ddd@yandex.ru
俄罗斯联邦, Yekaterinburg, 620999

A. Patselov

Mikheev Institute of Metal Physics, Ural Branch

Email: limon.5ddd@yandex.ru
俄罗斯联邦, Yekaterinburg, 620999

M. Ivanov

Kurdyumov Institute for Metal Physics

Email: limon.5ddd@yandex.ru
乌克兰, Kyiv, 03680

O. Slautin

Volgograd State Technical University

Email: limon.5ddd@yandex.ru
俄罗斯联邦, Volgograd, 400005

Yu. Besshaposhnikov

OAO Uralkhimmash

Email: limon.5ddd@yandex.ru
俄罗斯联邦, Yekaterinburg, 620010

补充文件

附件文件
动作
1. JATS XML

版权所有 © Allerton Press, Inc., 2016