Impact of long-term relaxation on the phase composition of Pd–5.3 at % In–0.5 at % Ru alloy after hydrogenation
- Autores: Akimova O.V.1, Avdyukhina V.M.1, Shchetinin I.V.2
-
Afiliações:
- Faculty of Physics
- Center for X-ray Diffraction
- Edição: Volume 80, Nº 12 (2016)
- Páginas: 1472-1475
- Seção: Proceedings of the VI International Conference “Crystal Physics and the Deformation Behavior of Promising Materials”
- URL: https://journals.rcsi.science/1062-8738/article/view/184907
- DOI: https://doi.org/10.3103/S1062873816120030
- ID: 184907
Citar
Resumo
The structural state of a hydrogenated foil of Pd 5.3 at %–In 0.5 at % Ru alloy with a long relaxation time (55000 h) is studied via X-ray diffraction. Changes in the phase composition of the alloy during relaxation after hydrogen escapes from it are established. The quasi-stability of the distribution of the widths of areas of coherent scattering (ACS) is revealed by the concentration of indium atoms in directions ≪100≫ and ≪111≫.
Sobre autores
O. Akimova
Faculty of Physics
Autor responsável pela correspondência
Email: akimova@physics.msu.ru
Rússia, Moscow, 119991
V. Avdyukhina
Faculty of Physics
Email: akimova@physics.msu.ru
Rússia, Moscow, 119991
I. Shchetinin
Center for X-ray Diffraction
Email: akimova@physics.msu.ru
Rússia, Moscow, 119049
Arquivos suplementares