Beneficiation of Oxidized Lead-Zinc Ores by Flotation Using Different Chemicals and Test Conditions


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

This study presents the recovery of oxide-carbonate lead-zinc ores using different chemical reagents under different test conditions by flotation. The run-of-mine oxide-carbonate Pb-Zn ore contains 9.05% Pb and 11.97% Zn with a major mineralization of smithsonite and cerussite. First experimental work was grinding tests to reduce -106 μm size fractions with two 15-minute grinding stages. Pre-flotation tests gave similar results for Pb, but neither pH, ZnSO4, CuSO4 nor collectors like AERO 3477, 3501 and 8651 made favorable effect on the recovery of Zn. Therefore, the studies were emphasized for recovering Pb concentrate by changing the amount of chemicals used, such as CMC, Na2S, AERO promotor. After six stage of flotation with 350 g/t KAX, 275 g/t AERO 407, 7500 g/t Na2S, 1000 g/t CMC, the concentration of 70.93% Pb with 71.56% recovery was achieved. The 91.51% Zinc remained in the tailing with 14.66% Zn grade.

Негізгі сөздер

Авторлар туралы

N. Mütevellioğlu

Sivas Cumhuriyet University, Department of Mining Engineering

Email: yekeler@cumhuriyet.edu.tr
Түркия, Sivas, 58140

M. Yekeler

Sivas Cumhuriyet University, Department of Mining Engineering

Хат алмасуға жауапты Автор.
Email: yekeler@cumhuriyet.edu.tr
Түркия, Sivas, 58140

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Pleiades Publishing, Inc., 2019