Sulphuric-Acid Leaching of Ural Oxidized Nickel Ore with Sodium Sulfite and Fluoride Additives


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

The process of leaching oxidized nickel ore in sulphuric acid with the additives of sodium sulfite and fluoride is investigated. Tochilnogorsky deposit ore (Sverdlovsk Region) is used to prove theoretically and experimentally efficient application of fluoride in dissociation of nickel minerals (nontronite and garnierite) in oxidized nickel ore. It is shown that at NaF consumption of 10 kg/t, it is possible to enhance maximum extraction of nickel to solution from 82.3–86.9 to 96.0–98.7% at the residual sulphuric acid concentration of 10–20 g/l in the working bath. It is found that the sodium fluoride additives lower the process activation energy from 22.8 to 12.9 kJ/mole. This means that the reaction of sulphuric-acid leaching proceeds in diffusion–kinetic mode and that sodium fluoride is applicable as the leaching accelerator.

作者简介

A. Klyushnikov

Uralmekhanobr—Research and Design Institution for Mineral Processing and Mechanical Conversion

编辑信件的主要联系方式.
Email: kl-anton-mih@yandex.ru
俄罗斯联邦, Yekaterinburg, 620144

补充文件

附件文件
动作
1. JATS XML

版权所有 © Pleiades Publishing, Ltd., 2018