Extraction of TiAl powder from SHS-produced TiAl–MgO semiproduct by treatment in different solutions
- Autores: Ignat’eva T.I.1, Vershinnikov V.I.1, Semenova V.N.1, Miloserdova O.M.1
-
Afiliações:
- Institute of Structural Macrokinetics and Materials Science
- Edição: Volume 26, Nº 2 (2017)
- Páginas: 115-118
- Seção: Article
- URL: https://journals.rcsi.science/1061-3862/article/view/195837
- DOI: https://doi.org/10.3103/S1061386217020066
- ID: 195837
Citar
Resumo
Explored was the extraction of target TiAl powder from SHS-produced TiAl–MgO semiproduct by treatment in acids (H2SO4, HCl,) and NH4Cl solution. Acid leaching was found to be accompanied by marked elution of target TiAl: the yield of TiAl powder was 21 and 33% in case of leaching with H2SO4 and HCl, respectively. But upon leaching with enriched NH4Cl solution at 70–80°C for 30 min, the yield of purified TiAl powder attained a value of 60%.
Palavras-chave
Sobre autores
T. Ignat’eva
Institute of Structural Macrokinetics and Materials Science
Autor responsável pela correspondência
Email: itian@ism.ac.ru
Rússia, Chernogolovka, Moscow, 142432
V. Vershinnikov
Institute of Structural Macrokinetics and Materials Science
Email: itian@ism.ac.ru
Rússia, Chernogolovka, Moscow, 142432
V. Semenova
Institute of Structural Macrokinetics and Materials Science
Email: itian@ism.ac.ru
Rússia, Chernogolovka, Moscow, 142432
O. Miloserdova
Institute of Structural Macrokinetics and Materials Science
Email: itian@ism.ac.ru
Rússia, Chernogolovka, Moscow, 142432
Arquivos suplementares