Extraction of TiAl powder from SHS-produced TiAl–MgO semiproduct by treatment in different solutions


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

Explored was the extraction of target TiAl powder from SHS-produced TiAl–MgO semiproduct by treatment in acids (H2SO4, HCl,) and NH4Cl solution. Acid leaching was found to be accompanied by marked elution of target TiAl: the yield of TiAl powder was 21 and 33% in case of leaching with H2SO4 and HCl, respectively. But upon leaching with enriched NH4Cl solution at 70–80°C for 30 min, the yield of purified TiAl powder attained a value of 60%.

作者简介

T. Ignat’eva

Institute of Structural Macrokinetics and Materials Science

编辑信件的主要联系方式.
Email: itian@ism.ac.ru
俄罗斯联邦, Chernogolovka, Moscow, 142432

V. Vershinnikov

Institute of Structural Macrokinetics and Materials Science

Email: itian@ism.ac.ru
俄罗斯联邦, Chernogolovka, Moscow, 142432

V. Semenova

Institute of Structural Macrokinetics and Materials Science

Email: itian@ism.ac.ru
俄罗斯联邦, Chernogolovka, Moscow, 142432

O. Miloserdova

Institute of Structural Macrokinetics and Materials Science

Email: itian@ism.ac.ru
俄罗斯联邦, Chernogolovka, Moscow, 142432

补充文件

附件文件
动作
1. JATS XML

版权所有 © Allerton Press, Inc., 2017