Аннотация

Reactive sintering of 2Ti–AlN mixtures at T = 1300°C for τ = 2 h in an argon atmosphere was used to prepare Ti2AlN containing below 1 wt % TiN and exhibiting a laminate structure typical of MAX compounds. At lower values of T and τ, the TiN content of products increased. Sintering in vacuum yielded a material containing up to 20 wt % TiN. Contrary to our expectations, mechanical activation of green blends was found to increase the TiN content of sintered materials, due to intensification of thermal dissociation of AlN and elimination of Al, which shifts equilibrium toward two-phase Ti2AlN–TiN composite. Relative density of green compacts was found to produce little or no influence on phase composition of products.

Негізгі сөздер

Авторлар туралы

M. Luginina

Institute of Structural Macrokinetics and Materials Science

Хат алмасуға жауапты Автор.
Email: m.luginina@gmail.com
Ресей, Moscow, 142432

D. Kovalev

Institute of Structural Macrokinetics and Materials Science

Email: m.luginina@gmail.com
Ресей, Moscow, 142432

A. Sytschev

Institute of Structural Macrokinetics and Materials Science

Email: m.luginina@gmail.com
Ресей, Moscow, 142432

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Allerton Press, Inc., 2016