Low-weight TiAl3 composites by thermal explosion


Citar

Texto integral

Acesso aberto Acesso aberto
Acesso é fechado Acesso está concedido
Acesso é fechado Somente assinantes

Resumo

Dispersion-strengthened TiAl3-based material with uniform structure and high compression strength (σc ≈ 850 MPa) was SHS-produced from Ti–Al–B4C blends in a mode of thermal explosion by using the B4C particles coated with a TiB2/TiC layer as a strengthening agent and preliminary mechanical activation of Ti–Al powder mixtures. The Ti + 3Al mixtures were mechanically activated in a planetary mill for 3 or 6 min and then 10 or 20 wt % of coated B4C particles were added. Pelleted samples were placed into a reaction chamber and heated in an electric furnace under Ar to a self-ignition temperature. The process was optimized and recommended for practical implementation.

Sobre autores

O. Kamynina

Institute of Structural Macrokinetics and Materials Science

Autor responsável pela correspondência
Email: kuz@ism.ac.ru
Rússia, Chernogolovka, Moscow, 142432

S. Vadchenko

Institute of Structural Macrokinetics and Materials Science

Email: kuz@ism.ac.ru
Rússia, Chernogolovka, Moscow, 142432

A. Sytschev

Institute of Structural Macrokinetics and Materials Science

Email: kuz@ism.ac.ru
Rússia, Chernogolovka, Moscow, 142432

I. Kovalev

Institute of Structural Macrokinetics and Materials Science

Email: kuz@ism.ac.ru
Rússia, Chernogolovka, Moscow, 142432

Arquivos suplementares

Arquivos suplementares
Ação
1. JATS XML

Declaração de direitos autorais © Allerton Press, Inc., 2016