Effect of temperature and charge stand on electrochemical performance of fiber Nickel–Cadmium cell


Citar

Texto integral

Acesso aberto Acesso aberto
Acesso é fechado Acesso está concedido
Acesso é fechado Somente assinantes

Resumo

The effect of temperature and charge stand periods on the discharge capacity of Nickel–Cadmium (Ni–Cd) cell is investigated quantitatively. 15 A h Ni–Cd cells with NiOOH cathode and Cd anode were used as test system. The cells were charged in two step constant current modes up to 1.7 V, then stored at different temperatures from–20 to 60°C for charge stand periods of 1 day, 7 days and 15 days and discharged at 1 С rate current until the cell voltage reached 1.0 V. Although the discharge capacity of these cells at and around room temperature i.e., 10 to 30°C is good, at temperatures below 0°C and above 40°C, the performance is poor. Also from 40 to 60°C, the discharge capacities decreased with charge stand periods due to self discharge and for sub ambient temperature decrease in capacity is minimal.

Sobre autores

M. Senthilkumar

Naval Science and Technological Laboratory

Autor responsável pela correspondência
Email: senthizhan@gmail.com
Índia, Visakhapatnam, 530027

K. Tanuja

Department of Chemical Engineering

Email: senthizhan@gmail.com
Índia, Visakhapatnam, 530003

T. Satyavani

Naval Science and Technological Laboratory

Email: senthizhan@gmail.com
Índia, Visakhapatnam, 530027

V. Ramesh Babu

Naval Science and Technological Laboratory

Email: senthizhan@gmail.com
Índia, Visakhapatnam, 530027

S. Naidu

Department of Chemical Engineering

Email: senthizhan@gmail.com
Índia, Visakhapatnam, 530003

Arquivos suplementares

Arquivos suplementares
Ação
1. JATS XML

Declaração de direitos autorais © Pleiades Publishing, Ltd., 2017