The influence of the composition of powder wire on the properties of the applied layer on steel samples is studied in the laboratory. If amorphous graphite in 35V9Kh3SF powder wire is replaced by material containing carbon and fluorine, the porosity of the applied layer is reduced, and fewer nonmetallic inclusions (including row oxide inclusions and undeformable silicates) are present. Statistical analysis of the experimental data illustrates the influence of the carbon equivalent of the 35V9Kh3SF powder wire on the hardness of the applied layer (including the mean surface hardness and the microhardness of martensite). With increase in the carbon equivalent calculated by the Paton Institute’s formula, the hardness of the applied layer linearly increases.

Об авторах

N. Kozyrev

Siberian State Industrial University

Автор, ответственный за переписку.
Email: Kozyrev_na@mtsp.sibsiu.ru
Россия, Novokuznetsk

N. Kibko

Siberian State Industrial University

Email: Kozyrev_na@mtsp.sibsiu.ru
Россия, Novokuznetsk

A. Umanskii

Siberian State Industrial University

Email: Kozyrev_na@mtsp.sibsiu.ru
Россия, Novokuznetsk

D. Titov

Siberian State Industrial University

Email: Kozyrev_na@mtsp.sibsiu.ru
Россия, Novokuznetsk

L. Bashchenko

Siberian State Industrial University

Email: Kozyrev_na@mtsp.sibsiu.ru
Россия, Novokuznetsk


© Allerton Press, Inc., 2016

Данный сайт использует cookie-файлы

Продолжая использовать наш сайт, вы даете согласие на обработку файлов cookie, которые обеспечивают правильную работу сайта.

О куки-файлах