The influence of the composition of powder wire on the properties of the applied layer on steel samples is studied in the laboratory. If amorphous graphite in 35V9Kh3SF powder wire is replaced by material containing carbon and fluorine, the porosity of the applied layer is reduced, and fewer nonmetallic inclusions (including row oxide inclusions and undeformable silicates) are present. Statistical analysis of the experimental data illustrates the influence of the carbon equivalent of the 35V9Kh3SF powder wire on the hardness of the applied layer (including the mean surface hardness and the microhardness of martensite). With increase in the carbon equivalent calculated by the Paton Institute’s formula, the hardness of the applied layer linearly increases.

Авторлар туралы

N. Kozyrev

Siberian State Industrial University

Хат алмасуға жауапты Автор.
Email: Kozyrev_na@mtsp.sibsiu.ru
Ресей, Novokuznetsk

N. Kibko

Siberian State Industrial University

Email: Kozyrev_na@mtsp.sibsiu.ru
Ресей, Novokuznetsk

A. Umanskii

Siberian State Industrial University

Email: Kozyrev_na@mtsp.sibsiu.ru
Ресей, Novokuznetsk

D. Titov

Siberian State Industrial University

Email: Kozyrev_na@mtsp.sibsiu.ru
Ресей, Novokuznetsk

L. Bashchenko

Siberian State Industrial University

Email: Kozyrev_na@mtsp.sibsiu.ru
Ресей, Novokuznetsk


© Allerton Press, Inc., 2016

Осы сайт cookie-файлдарды пайдаланады

Біздің сайтты пайдалануды жалғастыра отырып, сіз сайттың дұрыс жұмыс істеуін қамтамасыз ететін cookie файлдарын өңдеуге келісім бересіз.< / br>< / br>cookie файлдары туралы< / a>