Shanxi anthracite was subjected to oxygen-oxidation at 250°C in all aqueous solution of potassium hydroxide to produce solid benzene polycarboxylic acid (BPCA), and then the BPCA were selectively decarboxylated in the mixed medium of concentrated H2SO4 and KHSO4 to produce crude pyromellitic acid (PA). Pure PA was obtained by solvent recrystallization method, and the best solvent was 2-pentanone. Pure pyromellitic anhydride (PMDA) was gotton by heating pure pyromellitic acid in vacuum chamber at 260°C for 3 h. The remaining BPCA which through 2-pentanone recrystallization was isomerizated with consistent temperature at 420°C for 2 h. Appropriation pH of BPCA, initial pressure of carbon dioxide and cadmium carbonate catalyst were provided to produce crude terephthalic acid (TPA). Pure TPA was obtained by washing and drying the crude TPA precipitation.

作者简介

Kun Du

Department of Chemistry and Chemical Engineering

编辑信件的主要联系方式.
Email: kundu408@gmail.com
中国, Liupanshui, 553004

Yu Li

Department of Chemistry and Chemical Engineering

Email: kundu408@gmail.com
中国, Liupanshui, 553004

Lin Li

Department of Chemistry and Chemical Engineering

Email: kundu408@gmail.com
中国, Liupanshui, 553004

Hong Wu

Department of Chemistry and Chemical Engineering

Email: kundu408@gmail.com
中国, Liupanshui, 553004

补充文件

附件文件
动作
1. JATS XML

版权所有 © Allerton Press, Inc., 2016