New techniques for processing wastepaper


Citar

Texto integral

Acesso aberto Acesso aberto
Acesso é fechado Acesso está concedido
Acesso é fechado Somente assinantes

Resumo

The paper presents processing techniques of waste newsprint paper. Wastepaper was soaked in a soda or a hydrochloric solution and heated in a reactor with limited air access or in an autoclave. In the first stage, at 300°C, we obtained brittle carbonated coal with particle sizes of 10–50 µm, which can be used after milling as an additive in poor coals in the production of a coal-water slurry fuel. At the second stage, at 500–600°C, we obtained an amorphous carbon containing of up to 91.2% of C, which is widely used in the tire, rubber, and paint and varnish industries.

Sobre autores

G. Panasyuk

Kurnakov Institute of General and Inorganic Chemistry

Autor responsável pela correspondência
Email: panasyuk@igic.ras.ru
Rússia, Leninskii pr. 31, Moscow, 119991

L. Azarov

Kurnakov Institute of General and Inorganic Chemistry

Email: panasyuk@igic.ras.ru
Rússia, Leninskii pr. 31, Moscow, 119991

I. Voroshilov

Kurnakov Institute of General and Inorganic Chemistry

Email: panasyuk@igic.ras.ru
Rússia, Leninskii pr. 31, Moscow, 119991

V. Belan

Kurnakov Institute of General and Inorganic Chemistry

Email: panasyuk@igic.ras.ru
Rússia, Leninskii pr. 31, Moscow, 119991

I. Kozerozhets

Kurnakov Institute of General and Inorganic Chemistry

Email: panasyuk@igic.ras.ru
Rússia, Leninskii pr. 31, Moscow, 119991

E. Semenov

Kurnakov Institute of General and Inorganic Chemistry

Email: panasyuk@igic.ras.ru
Rússia, Leninskii pr. 31, Moscow, 119991

V. Stolyarova

Kurnakov Institute of General and Inorganic Chemistry

Email: panasyuk@igic.ras.ru
Rússia, Leninskii pr. 31, Moscow, 119991

A. Izotov

Kurnakov Institute of General and Inorganic Chemistry

Email: panasyuk@igic.ras.ru
Rússia, Leninskii pr. 31, Moscow, 119991

Arquivos suplementares

Arquivos suplementares
Ação
1. JATS XML

Declaração de direitos autorais © Pleiades Publishing, Ltd., 2016