Fatigue strength of a Ti–6Al–4V alloy produced by selective laser melting


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

The fatigue properties and the fracture mechanisms of the Ti–6Al–4V alloy produced by selective laser melting (SLM) from a powder of an CL41TiELI titanium alloy have been studied. Cylindrical blanks were grown at angles of 90° and 45° to a platform. The best fatigue strength is observed in the samples the blanks of which were grown at an angle of 45°. It is found that the structure of the SLM material can contain portions with unmelted powder particles, which are the places of initiation of fatigue cracks.

作者简介

M. Gerov

AO Corporation Moscow Heat Engineering Institute MIT

编辑信件的主要联系方式.
Email: zodom@mail.ru
俄罗斯联邦, alleya Berezovaya 10, Moscow, 127273

E. Vladislavskaya

AO Corporation Moscow Heat Engineering Institute MIT

Email: fatig@mail.ru
俄罗斯联邦, alleya Berezovaya 10, Moscow, 127273

V. Terent’ev

Baikov Institute of Metallurgy and Materials Science

编辑信件的主要联系方式.
Email: fatig@mail.ru
俄罗斯联邦, Leninskii pr. 49, Moscow, 119991

D. Prosvirnin

Baikov Institute of Metallurgy and Materials Science

Email: fatig@mail.ru
俄罗斯联邦, Leninskii pr. 49, Moscow, 119991

A. Kolmakov

Baikov Institute of Metallurgy and Materials Science

Email: fatig@mail.ru
俄罗斯联邦, Leninskii pr. 49, Moscow, 119991

O. Antonova

Baikov Institute of Metallurgy and Materials Science

Email: fatig@mail.ru
俄罗斯联邦, Leninskii pr. 49, Moscow, 119991


版权所有 © Pleiades Publishing, Ltd., 2016
##common.cookie##