The degassing from a hydrogen-saturated E125 zirconium alloy is studied as a function of its deformation. Zirconium alloy samples are subjected to tension at a relative elongation of 2.5, 5, and 10%. Undeformed and deformed samples were saturated with hydrogen by a galvanic method at a current density of 0.5 A/cm2; that is, they are hydrogen saturated and then deformed. As a result, the defects at which hydrogen is trapped in zirconium are identified. The quantity of hydrogen trapped by defects depends on the strain and the sequence of deformation and hydrogen saturation. This is a technical result of the investigations, which can be used to find optimum operation conditions for hydrogen-saturated zirconium articles.

作者简介

Yu. Tyurin

National Research Tomsk Polytechnic University

编辑信件的主要联系方式.
Email: tyurin@tpu.ru
俄罗斯联邦, pr. Lenina 30, Tomsk, 634050

V. Larionov

National Research Tomsk Polytechnic University

Email: tyurin@tpu.ru
俄罗斯联邦, pr. Lenina 30, Tomsk, 634050

N. Nikitenkov

National Research Tomsk Polytechnic University

Email: tyurin@tpu.ru
俄罗斯联邦, pr. Lenina 30, Tomsk, 634050


版权所有 © Pleiades Publishing, Ltd., 2016
##common.cookie##