Effect of the Conditions of Machine Hidden Arc Welding with an Additional Hot Additive (Flux-Cored Electrode) on the Formation of a Joint Weld


Цитировать

Полный текст

Открытый доступ Открытый доступ
Доступ закрыт Доступ предоставлен
Доступ закрыт Только для подписчиков

Аннотация

The influence of the parameters of feeding and heating of an additional flux-cored electrode during machine hidden arc welding with an additional hot additive on the process is considered. Beads are deposited onto a 10-mm-thick steel (St3sp steel, GOST 380) plate, and the addition conditions, namely, the distance between the flux-cored electrode and the filler wire and the filler wire feed rate, are varied. The filler wire feed rate is found to depend on the electric current used for heating and to be independent of the distance between the point of introduction of the additional hot additive and the main arc. The limiting amount of the filler wire additive at which the transition from a deposited metal to the base metal is not sharp is determined.

Об авторах

N. Kobernik

FGAU NUTsSK, Bauman Moscow State Technical University

Email: galcomputer@mail.ru
Россия, Moscow

R. Mikheev

FGAU NUTsSK, Bauman Moscow State Technical University

Email: galcomputer@mail.ru
Россия, Moscow

A. Linnik

FGAU NUTsSK, Bauman Moscow State Technical University

Email: galcomputer@mail.ru
Россия, Moscow

A. Pankratov

FGAU NUTsSK, Bauman Moscow State Technical University

Email: galcomputer@mail.ru
Россия, Moscow

V. Brovko

FGAU NUTsSK, Bauman Moscow State Technical University

Email: galcomputer@mail.ru
Россия, Moscow

A. Galinovskii

Bauman Moscow State Technical University

Автор, ответственный за переписку.
Email: galcomputer@mail.ru
Россия, Moscow


© Pleiades Publishing, Ltd., 2018

Данный сайт использует cookie-файлы

Продолжая использовать наш сайт, вы даете согласие на обработку файлов cookie, которые обеспечивают правильную работу сайта.

О куки-файлах