The influence of the parameters of feeding and heating of an additional flux-cored electrode during machine hidden arc welding with an additional hot additive on the process is considered. Beads are deposited onto a 10-mm-thick steel (St3sp steel, GOST 380) plate, and the addition conditions, namely, the distance between the flux-cored electrode and the filler wire and the filler wire feed rate, are varied. The filler wire feed rate is found to depend on the electric current used for heating and to be independent of the distance between the point of introduction of the additional hot additive and the main arc. The limiting amount of the filler wire additive at which the transition from a deposited metal to the base metal is not sharp is determined.

Авторлар туралы

N. Kobernik

FGAU NUTsSK, Bauman Moscow State Technical University

Email: galcomputer@mail.ru
Ресей, Moscow

R. Mikheev

FGAU NUTsSK, Bauman Moscow State Technical University

Email: galcomputer@mail.ru
Ресей, Moscow

A. Linnik

FGAU NUTsSK, Bauman Moscow State Technical University

Email: galcomputer@mail.ru
Ресей, Moscow

A. Pankratov

FGAU NUTsSK, Bauman Moscow State Technical University

Email: galcomputer@mail.ru
Ресей, Moscow

V. Brovko

FGAU NUTsSK, Bauman Moscow State Technical University

Email: galcomputer@mail.ru
Ресей, Moscow

A. Galinovskii

Bauman Moscow State Technical University

Хат алмасуға жауапты Автор.
Email: galcomputer@mail.ru
Ресей, Moscow


© Pleiades Publishing, Ltd., 2018

Осы сайт cookie-файлдарды пайдаланады

Біздің сайтты пайдалануды жалғастыра отырып, сіз сайттың дұрыс жұмыс істеуін қамтамасыз ететін cookie файлдарын өңдеуге келісім бересіз.< / br>< / br>cookie файлдары туралы< / a>