Refining a complex ZhS32-VI nickel alloy from silicon and phosphorus by unidirectional solidification of the melt at low solidification front velocities
- Авторы: Sidorov V.1, Kablov D.1, Min P.1, Vadeev V.1
-
Учреждения:
- All-Russian Scientific Research Institute of Aviation Materials
- Выпуск: Том 2016, № 13 (2016)
- Страницы: 1221-1226
- Раздел: Processes of Manufacture of Ferrous and Nonferrous Metals
- URL: https://journals.rcsi.science/0036-0295/article/view/171117
- DOI: https://doi.org/10.1134/S003602951613019X
- ID: 171117
Цитировать
Аннотация
The possibility of decreasing the silicon and phosphorus contents in a high-temperature ZhS32-VI nickel alloy by directional movement of solidification front at a velocity V = 6 mm/h has been studied. As a result, the contents of the impurities have decreased as compared to those in the starting alloy; the decrease in the silicon and phosphorus contents is from 2 to 4 and from 14 to 20 times, respectively. Thus, nonmetallic inclusions, in particular, those containing silicon and phosphorus, are moved to the top of the ingot.
Ключевые слова
Об авторах
V. Sidorov
All-Russian Scientific Research Institute of Aviation Materials
Email: viamlab3@mail.ru
Россия, Moscow, 105005
D. Kablov
All-Russian Scientific Research Institute of Aviation Materials
Email: viamlab3@mail.ru
Россия, Moscow, 105005
P. Min
All-Russian Scientific Research Institute of Aviation Materials
Автор, ответственный за переписку.
Email: viamlab3@mail.ru
Россия, Moscow, 105005
V. Vadeev
All-Russian Scientific Research Institute of Aviation Materials
Email: viamlab3@mail.ru
Россия, Moscow, 105005