Refining a complex ZhS32-VI nickel alloy from silicon and phosphorus by unidirectional solidification of the melt at low solidification front velocities
- Авторлар: Sidorov V.1, Kablov D.1, Min P.1, Vadeev V.1
-
Мекемелер:
- All-Russian Scientific Research Institute of Aviation Materials
- Шығарылым: Том 2016, № 13 (2016)
- Беттер: 1221-1226
- Бөлім: Processes of Manufacture of Ferrous and Nonferrous Metals
- URL: https://journals.rcsi.science/0036-0295/article/view/171117
- DOI: https://doi.org/10.1134/S003602951613019X
- ID: 171117
Дәйексөз келтіру
Аннотация
The possibility of decreasing the silicon and phosphorus contents in a high-temperature ZhS32-VI nickel alloy by directional movement of solidification front at a velocity V = 6 mm/h has been studied. As a result, the contents of the impurities have decreased as compared to those in the starting alloy; the decrease in the silicon and phosphorus contents is from 2 to 4 and from 14 to 20 times, respectively. Thus, nonmetallic inclusions, in particular, those containing silicon and phosphorus, are moved to the top of the ingot.
Негізгі сөздер
Авторлар туралы
V. Sidorov
All-Russian Scientific Research Institute of Aviation Materials
Email: viamlab3@mail.ru
Ресей, Moscow, 105005
D. Kablov
All-Russian Scientific Research Institute of Aviation Materials
Email: viamlab3@mail.ru
Ресей, Moscow, 105005
P. Min
All-Russian Scientific Research Institute of Aviation Materials
Хат алмасуға жауапты Автор.
Email: viamlab3@mail.ru
Ресей, Moscow, 105005
V. Vadeev
All-Russian Scientific Research Institute of Aviation Materials
Email: viamlab3@mail.ru
Ресей, Moscow, 105005
![](/img/style/loading.gif)