Normalization of the Cold Shortness of Plate Steel: II. Short-Brittleness Thresholds in Pipe Tests


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

The following serial curves are obtained for a pipe steel of strength class K65 (Kh80): strength and plasticity curves during tension in the temperature range from–80 to +20°C, fracture energy from drop weight tear test (DWTT) diagrams, and impact toughness KCV curves (from–180 to +20°C). The ductile–brittle transition temperature range determined from the DWTT energy is shown to be higher than that determined from a KCV diagram by 80 K. The KCV–40 criterion is concluded to be more reliable than the DWTT–20 criterion. KCV and DWTT tests are shown to reproduce the crack starting conditions in a pipe, and the resistance of a high-strength pipe steel to extended fracture should be estimated using other criteria.

Авторлар туралы

M. Shtremel’

National University of Science and Technology MISiS

Хат алмасуға жауапты Автор.
Email: str@mfp.misis.ru
Ресей, Moscow, 119049

A. Arabei

PAO Gazprom

Email: str@mfp.misis.ru
Ресей, Moscow, 117997

A. Glebov

National University of Science and Technology MISiS

Email: str@mfp.misis.ru
Ресей, Moscow, 119049

I. Pyshmintsev

OAO PosNITI

Email: str@mfp.misis.ru
Ресей, Chelyabinsk, 454139

T. Esiev

OOO Gazprom VNIIGAZ

Email: str@mfp.misis.ru
Ресей, Moscow, 115583

A. Abakumov

FGUP RFYaTs-VNIIEF

Email: str@mfp.misis.ru
Ресей, Sarov, 607188


© Pleiades Publishing, Ltd., 2018

Осы сайт cookie-файлдарды пайдаланады

Біздің сайтты пайдалануды жалғастыра отырып, сіз сайттың дұрыс жұмыс істеуін қамтамасыз ететін cookie файлдарын өңдеуге келісім бересіз.< / br>< / br>cookie файлдары туралы< / a>