The macrokinetic regularities of the reactivity of synthesized Ni–Re (20 and 60 wt %) alloys in a sulfuric acid solution (100 g/L, 25–40°C) during direct current polarization are studied using physicochemical methods. The phase composition of the synthesized alloys is determined by the formation of solid solutions as a function of the initial Ni/Re weight ratio. These are two types of nickel solid solutions (Ni16Re0.2 and Ni14Re0.9) and one rhenium solution (Ni1.1Re). These solid solutions are anodically oxidized in the sequence of their structural rearrangement Ni16Re0.2 → Ni14Re0.9 → Ni1.1Re with a combined transition of the metals into an electrolyte solution. These solid solutions provide the reduction of Ni3+ to Ni2+ due to the depolarization ability of rhenium, being their component.

Авторлар туралы

V. Bryukvin

Baikov Institute of Metallurgy and Materials Science

Хат алмасуға жауапты Автор.
Email: brukvin@imet.ac.ru
Ресей, Leninskii pr. 49, Moscow, 119991

T. Elemesov

Baikov Institute of Metallurgy and Materials Science

Email: brukvin@imet.ac.ru
Ресей, Leninskii pr. 49, Moscow, 119991

O. Levchuk

Baikov Institute of Metallurgy and Materials Science

Email: brukvin@imet.ac.ru
Ресей, Leninskii pr. 49, Moscow, 119991

A. Bol’shikh

Baikov Institute of Metallurgy and Materials Science

Email: brukvin@imet.ac.ru
Ресей, Leninskii pr. 49, Moscow, 119991


© Pleiades Publishing, Ltd., 2016

Осы сайт cookie-файлдарды пайдаланады

Біздің сайтты пайдалануды жалғастыра отырып, сіз сайттың дұрыс жұмыс істеуін қамтамасыз ететін cookie файлдарын өңдеуге келісім бересіз.< / br>< / br>cookie файлдары туралы< / a>