The parameters of plasma–arc reduction melting of a charge of the carbon-containing leucoxene concentrate from the Yareg deposit are calculated, and the experimental data obtained on the basis of the calculated parameters are presented. Synthetic rutile with 3–4% silicon was synthesized.

About the authors

A. A. Nikolaev

Baikov Institute of Metallurgy and Materials Science

Author for correspondence.
Email: dym2004@bk.ru
Russian Federation, Leninskii pr. 49, Moscow, 119991

D. E. Kirpichev

Baikov Institute of Metallurgy and Materials Science

Email: dym2004@bk.ru
Russian Federation, Leninskii pr. 49, Moscow, 119991

A. V. Samokhin

Baikov Institute of Metallurgy and Materials Science

Email: dym2004@bk.ru
Russian Federation, Leninskii pr. 49, Moscow, 119991

A. V. Nikolaev

Baikov Institute of Metallurgy and Materials Science

Email: dym2004@bk.ru
Russian Federation, Leninskii pr. 49, Moscow, 119991


Copyright (c) 2016 Pleiades Publishing, Ltd.

This website uses cookies

You consent to our cookies if you continue to use our website.

About Cookies