Production, structure, texture, and mechanical properties of severely deformed magnesium


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

Methods of the severe plastic deformation (SPD) of pure magnesium at room temperature, namely, transverse extrusion and hydroextrusion in a self-destroyed shell, have been developed. The maximum true strain of the samples after the hydroextrusion was e ~ 3.2; in the course of transverse extrusion and subsequent cold rolling, a true strain of e ~ 6.0 was achieved. The structure and mechanical properties of the magnesium samples have been studied in different structural states. It has been shown that the SPD led to a decrease in the grain size d to ~2 μm; the relative elongation at fracture δ increased to ~20%. No active twinning has been revealed. The reasons for the high plasticity of magnesium after SPD according to the deformation modes suggested are discussed from the viewpoint of the hierarchy of the observed structural states.

Авторлар туралы

A. Volkov

Institute of Metal Physics, Ural Branch

Хат алмасуға жауапты Автор.
Email: volkov@imp.uran.ru
Ресей, ul. S. Kovalevskoi 18, Ekaterinburg, 620990

O. Antonova

Institute of Metal Physics, Ural Branch

Email: volkov@imp.uran.ru
Ресей, ul. S. Kovalevskoi 18, Ekaterinburg, 620990

B. Kamenetskii

Institute of Metal Physics, Ural Branch

Email: volkov@imp.uran.ru
Ресей, ul. S. Kovalevskoi 18, Ekaterinburg, 620990

I. Klyukin

Institute of Metal Physics, Ural Branch

Email: volkov@imp.uran.ru
Ресей, ul. S. Kovalevskoi 18, Ekaterinburg, 620990

D. Komkova

Institute of Metal Physics, Ural Branch

Email: volkov@imp.uran.ru
Ресей, ul. S. Kovalevskoi 18, Ekaterinburg, 620990

B. Antonov

Institute of High-Temperature Electrochemistry, Ural Branch

Email: volkov@imp.uran.ru
Ресей, ul. Akademicheskaya 20, Ekaterinburg, 620137

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Pleiades Publishing, Ltd., 2016