Structure, phase composition, and strengthening of cast Al–Ca–Mg–Sc alloys


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

The structure and phase composition of Al–Ca–Mg–Sc alloys containing 0.3 wt % Sc, up to 10 wt % Ca, and up to 10 wt % Mg have been investigated in the cast state and state after heat treatment. It has been shown that only binary phases Al4Ca, Al3Sc, and Al3Mg2 can be in equilibrium with the aluminum solid solution. It has been found that the maximum strengthening effect caused by the precipitation of Al3Sc nanoparticles for all investigated alloys is attained after annealing at 300–350°C.

Авторлар туралы

N. Belov

Department of Casting Process Technologies

Хат алмасуға жауапты Автор.
Email: nikolay-belov@yandex.ru
Ресей, Leninsky pr. 4, Moscow, 119049

E. Naumova

Department of Materials Science

Email: nikolay-belov@yandex.ru
Ресей, ul. Vtoraya Baumanskaya 5, Moscow, 105005

T. Bazlova

Department of Casting Process Technologies

Email: nikolay-belov@yandex.ru
Ресей, Leninsky pr. 4, Moscow, 119049

E. Alekseeva

Department of Casting Process Technologies

Email: nikolay-belov@yandex.ru
Ресей, Leninsky pr. 4, Moscow, 119049

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Pleiades Publishing, Ltd., 2016