Protection of Steel From Corrosive Wear in Water
- Autores: Logachev K.A.1, Guzenkova A.S.2, Ivanov S.S.1, Guzenkov S.A.1
-
Afiliações:
- Moscow State University of Mechanical Engineering (MAMI)
- National Research University – Higher School of Economics (NIU VShE)
- Edição: Volume 60, Nº 3-4 (2016)
- Páginas: 296-298
- Seção: Article
- URL: https://journals.rcsi.science/0026-0894/article/view/238351
- DOI: https://doi.org/10.1007/s11015-016-0289-4
- ID: 238351
Citar
Resumo
A gravimetric method is used to study corrosive wear of a test specimen – counterbody pair made of steel 40X in running water with pH 7.6 containing (g/liter): Ca2+ 0.035, Mg2+ 0.016, Cl– 0.023, SO42 – 0.039, with addition of alizarin oil (AO). It is established that AO in running water reduces the amount of corrosive wear in the load range 4.8–20.2 kg, and as load increases the protective effect of AO decreases from 52.4 to 1%.
Sobre autores
K. Logachev
Moscow State University of Mechanical Engineering (MAMI)
Autor responsável pela correspondência
Email: gigrafor123@mail.ru
Rússia, Moscow
A. Guzenkova
National Research University – Higher School of Economics (NIU VShE)
Email: gigrafor123@mail.ru
Rússia, Moscow
S. Ivanov
Moscow State University of Mechanical Engineering (MAMI)
Email: gigrafor123@mail.ru
Rússia, Moscow
S. Guzenkov
Moscow State University of Mechanical Engineering (MAMI)
Email: gigrafor123@mail.ru
Rússia, Moscow
Arquivos suplementares