A method of heat treatment of DI37-VI steel exhibiting precipitation hardening is developed with due allowance for the steel microstructure and with determining the chemical composition of carbides and the matrix after each operation. In the case of low-temperature tempering, the mechanical properties of steel are found to be little different from its properties obtained by means of multiple high-temperature tempering (ageing); in the latter case, however, the wear resistance of steel in the case of cutting of steel bars is 1.5 times higher. It is demonstrated that the wear resistance of steel is significantly affected by the chemical composition of carbides and the matrix.

Авторлар туралы

O. Stoyanovskii

Design and Technology Division of the Lavrentyev Institute of Hydrodynamics, Siberian Branch

Хат алмасуға жауапты Автор.
Email: stn@sibexplo.com
Ресей, Novosibirsk, 630090

A. Maznichevskii

Limited Liability Company “Laboratory of Special Metallurgy” (Lasmet)

Email: stn@sibexplo.com
Ресей, Chelyabinsk, 454047

A. Pikarevskii

Design and Technology Division of the Lavrentyev Institute of Hydrodynamics, Siberian Branch

Email: stn@sibexplo.com
Ресей, Novosibirsk, 630090

E. Vasyukova

Limited Liability Company “Laboratory of Special Metallurgy” (Lasmet)

Email: stn@sibexplo.com
Ресей, Chelyabinsk, 454047

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Pleiades Publishing, Ltd., 2018