Optimization of the Carbosilicothermic Synthesis of the Ti4SiC3 MAX Phase


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

We have studied the formation of the Ti4SiC3 MAX phase during the vacuum carbosilicothermic reduction of TiO2 with a combined reducing agent consisting of SiC and elemental Si and analyzed the effects of the synthesis temperature, heat treatment time, and percentage of elemental silicon in the starting mixture on the Ti4SiC3 yield. Optimal Ti4SiC3 synthesis conditions are as follows: temperature from 1550 to 1650°C, isothermal holding time of 360 min, and the starting-mixture composition TiO2 + 1.2SiC + 0.6Si. The Ti4SiC3 yield then reaches 92 wt %.

作者简介

E. Istomina

Institute of Chemistry, Komi Scientific Center, Ural Branch

编辑信件的主要联系方式.
Email: istomina-ei@yandex.ru
俄罗斯联邦, Pervomaiskaya ul. 48, Syktyvkar, Komi Republic, 167982

P. Istomin

Institute of Chemistry, Komi Scientific Center, Ural Branch

Email: istomina-ei@yandex.ru
俄罗斯联邦, Pervomaiskaya ul. 48, Syktyvkar, Komi Republic, 167982

A. Nadutkin

Institute of Chemistry, Komi Scientific Center, Ural Branch

Email: istomina-ei@yandex.ru
俄罗斯联邦, Pervomaiskaya ul. 48, Syktyvkar, Komi Republic, 167982

V. Grass

Institute of Chemistry, Komi Scientific Center, Ural Branch

Email: istomina-ei@yandex.ru
俄罗斯联邦, Pervomaiskaya ul. 48, Syktyvkar, Komi Republic, 167982

A. Bogdanova

Syktyvkar State University

Email: istomina-ei@yandex.ru
俄罗斯联邦, Oktyabr’skii pr. 55, Syktyvkar, Komi Republic, 167001

补充文件

附件文件
动作
1. JATS XML

版权所有 © Pleiades Publishing, Ltd., 2018