Effect of Si additions on the microstructure and mechanical properties of hot-pressed B4C
- Авторлар: Perevislov S.N.1, Lysenkov A.S.2, Vikhman S.V.3
-
Мекемелер:
- Central Research Institute of Materials
- Baikov Institute of Metallurgy and Materials Science
- St. Petersburg State Technological Institute (Technical University)
- Шығарылым: Том 53, № 4 (2017)
- Беттер: 376-380
- Бөлім: Article
- URL: https://journals.rcsi.science/0020-1685/article/view/158199
- DOI: https://doi.org/10.1134/S0020168517040148
- ID: 158199
Дәйексөз келтіру
Аннотация
Dense B4C-based materials containing up to 4.9 wt % Si have been produced by hot pressing in the temperature range 1600–1700°C. In this process, the silicon melts to form a liquid phase, which improves the sinterability of the material. The boron carbide partially dissolves in the liquid Si to form silicon carbide between the B4C grains. The relative density, bending strength, Vickers hardness, and fracture toughness of the materials obtained in this study are 99.0 ± 0.1%, 584 ± 12 MPa, 39.4 ± 0.1 GPa, and 5.3 ± 0.2 MPa m1/2, respectively. The materials experience predominantly transcrystalline fracture.
Негізгі сөздер
Авторлар туралы
S. Perevislov
Central Research Institute of Materials
Хат алмасуға жауапты Автор.
Email: perevislov@mail.ru
Ресей, Paradnaya ul. 8, St. Petersburg, 191014
A. Lysenkov
Baikov Institute of Metallurgy and Materials Science
Email: perevislov@mail.ru
Ресей, Leninskii pr. 49, Moscow, 119991
S. Vikhman
St. Petersburg State Technological Institute (Technical University)
Email: perevislov@mail.ru
Ресей, Moskovskii pr. 26, St. Petersburg, 190013
Қосымша файлдар