Аннотация

We have studied the structural properties of the phase K1.2Cu0.4Fe2O4 and the effect of potassium on its catalytic activity for oxidation of carbon. The results demonstrate that the potassium-doped phase differs from the undoped ferrite CuFe2O4 in linear dimensions of its unit cell, high density of structural defects, and low-temperature activity and activation energy for the catalytic process. Contact interaction between K1.2Cu0.4Fe2O4 and carbon in the temperature range 240–420°C leads to the reduction of Cu2+ to Cu+ and the formation of Cu2O, CuFeO2, and K2Fe4O7. Testing results for the phases identified indicate that the catalytic processes in the presence of K2Fe4O7 and K1.2Cu0.4Fe2O4 are identical.

Авторлар туралы

N. Lebukhova

Institute of Materials Science, Khabarovsk Scientific Center, Far East Branch

Email: pal_chig@mail.ru
Ресей, Tikhookeanskaya ul. 153, Khabarovsk, 680042

P. Chigrin

Institute of Materials Science, Khabarovsk Scientific Center, Far East Branch

Хат алмасуға жауапты Автор.
Email: pal_chig@mail.ru
Ресей, Tikhookeanskaya ul. 153, Khabarovsk, 680042

E. Kirichenko

Institute of Materials Science, Khabarovsk Scientific Center, Far East Branch

Email: pal_chig@mail.ru
Ресей, Tikhookeanskaya ul. 153, Khabarovsk, 680042

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Pleiades Publishing, Ltd., 2016