Effect of synthesis conditions on the particle size and luminescence properties of the La3.16Gd10Yb0.7Er0.14Ge2B6O34 germanate borate


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

La3.16Gd10Yb0.7Er0.14Ge2B6O34 germanate borates have been synthesized using liquid-phase homogenization of starting materials. The smallest crystallite size, 25.3 ± 0.8 nm, has been obtained using a combination of two complexing agents (citric acid and mannitol). We have determined the energy yield of upconversion luminescence in the synthesized borates. Using tartaric acid as a complexing agent, we have obtained a phosphor with an energy yield of upconversion luminescence Ben = 0.52% (λex = 974 nm, P = 2.5 W/cm2) and crystallite size of 80.6 ± 0.5 nm.

作者简介

V. Krut’ko

Kurnakov Institute of General and Inorganic Chemistry

编辑信件的主要联系方式.
Email: kroutko@igic.ras.ru
俄罗斯联邦, Leninskii pr. 31, Moscow, 119991

M. Komova

Kurnakov Institute of General and Inorganic Chemistry

Email: kroutko@igic.ras.ru
俄罗斯联邦, Leninskii pr. 31, Moscow, 119991

D. Pominova

Prokhorov General Physics Institute

Email: kroutko@igic.ras.ru
俄罗斯联邦, ul. Vavilova 38, Moscow, 119991

A. Yaroslavtsev

Kurnakov Institute of General and Inorganic Chemistry

Email: kroutko@igic.ras.ru
俄罗斯联邦, Leninskii pr. 31, Moscow, 119991

补充文件

附件文件
动作
1. JATS XML

版权所有 © Pleiades Publishing, Ltd., 2016